Dental glass ceramics, main ingredients are Lithium Disilicate, through special process. Bending strength The average biaxial bending strength after being fully crystallized is 637Mpa, higher than the standard strength value, set by ISO6892:2008 For Dental...
Mixing resin with zirconia significantly improves the wear resistance of composite ceramics. Due to its simple and rapid crystallization process, as well as its ultra-high aesthetic repair effect, it is chosen as a high-strength CAD repair material.